Main Raw Material: | Silicone | Other Names: | Silicone Glue |
---|---|---|---|
Color: | White&grey | Classification: | Double Components Adhesives |
Usage: | Construction, Fiber & Garment, Construction, Fiber & Garment, Computer | Viscosity: | 68 CPS |
Thermal Conductivity: | 2-5.5 W/m-K | Weight: | 1 Kg/can, 10kg/barrel |
Highlight: | 10kg thermal conductive silicone grease,5.5W/m.K thermal contact paste,10kg Thermal Compound Grease |
Thermal Conductivity Silicone Grease Thermal Compound Grease30g/1kg/10kg
Product Description
Thermall conductive silicone grease is a grease-like silicone material, heavily filled with heat conductive metal oxides. This combination promotes high thermal conductivity, low bleed and high-temperature stability.
The compound resists changes in con-sistency at temperatures up to approxi-mately 350°F (177°C). In doing so, it helps maintain a positive heat sink seal to improve heat transfer from the electrical/electronic device to the heat sink or chassis, thereby increasing overall efficiency of the device.
keywords:Excellent Thermal Conductivity Silicone Grease For Telecom Equipment
Features
• High thermal conductivity
• Low bleed
• Stable at high temperatures
Composition
Greaselike silicone fluid thickened with metal oxide filler
Application areas
Thermal grease is widely used in electronics, electrical appliances, passive components of the heat, filling or coating to derive the heat generated by components. Such as CPU and radiator caulking, high-power transistors, thyristor components, diodes and substrate (aluminum, copper) at the gap between the filling, power tubes and heatsinks, semiconductor cooling, reducing heating element Operating temperature.
Typical Properties
Method |
Test |
Unit |
Result |
/ |
Color |
/ |
White |
ASTM D 217 |
Consistency, Penetration |
/ |
|
/ |
unworked |
/ |
300 |
/ |
worked 60 strokes |
/ |
275 |
/ |
worked 100,000 strokes |
/ |
245 |
Fed. Std. 791, Bleed after 24 hr at 392°F (200°C) |
Method 321.2 |
percent |
0.05 |
Fed. Std. 791, Evaporation after 24 hr at 392°F (200°C) |
Method 321.2 |
percent |
0.5 |
ASTM D 2265 |
Drop Point |
°F (°C) |
570 (300) |
ASTM D 1475 |
Specific Gravity at 77°F (25°C) |
/ |
2.1 |
CTM1 0069 |
Thermal Conductivity, K Factor |
cal/sec-cm-°C |
0.0014 |
ASTM D 149 |
Dielectric Strength2 |
volts/mil |
210 |
ASTM D 495 |
Arc Resistance |
seconds |
165 |
ASTM D 150 Dielectric Constant, |
|||
/ |
at 100 Hz |
/ |
5 |
/ |
at 100 kHz |
/ |
5 |
ASTM D 150 Dissipation Factor, |
|||
/ |
at 100 Hz |
/ |
0.01 |
/ |
at 100 kHz |
/ |
0.02 |
ASTM D 1169 |
Volume Resistivity |
ohm-cm |
2 x 1015 |
ASTM D 4049 |
Water Spray Off |
percent |
1.3 |
Packing & Shipping
A1:All the data in the sheet tested out by the third partly,ASTM D5470 is utilized to test the thermal conductivity.
Q2:How to find a right thermal conductivity for my application?
Q4:Do you offer free samples?
A4:Yes,we are willing to offer free sample but pls kindly note that your side pay for freight.
Q5:How to ship the orders?
A5:We will help to arrange transportation dor you.If you want to use your own courier account pls kindly tell us before shipping out.
Q6:What's the lead time?
A6:Sample order costs 1~3 workdays and 3~5 workdays for production.